View Single Post

Old June 21st, 11:17 AM   #7 (permalink)
bri91xj
Elite Member
 
Join Date: Mar 2004
Location: Ohio
Posts: 43
lead?

i was working off two sets of instructions, one said to use a piece of lead, other said to use the foil. So i'l try the Titanium wire next time. And would lead work too?
Is about 20 mins long enough to keep it i nthe bath?
I did a stock spyder body with factory anno on it. i read later that it wont conduct electricity with that layer, but the acid bath romoved it, so i sanded it down again and it should be ready for next time.
And i'll buy a new charger, what size wire is good to use?
i have a really thick Aliminum wire right now,